Nonwoven Fabrics Polyester Spunbond Carbon Fiber in Industrial Filtration
Properties |
Unit |
Specifications |
Notes |
Main ingredients |
— |
Polyester + Carbon Fiber |
|
Weight/Tolerance |
g/m2 |
130±12 |
ISO 9864 |
Post-processing |
— |
/ |
|
Thickness |
mm |
0.4±0.05 |
ISO 9073 |
Air permeability |
mm/s |
>620 |
ISO 9237(△P=200Pa) |
Working temperature |
℃ |
100 |
|
Max. Operation temperature |
℃ |
120 |
|
Tensile strength/ MD |
N/5cm |
>380 |
ISO 9073 |
Tensile strength/CD |
N/5cm |
>280 |
ISO 9073 |
Elongation/MD |
% |
>20 |
ISO 9073 |
Elongation/CD |
% |
>20 |
ISO 9073 |
Surface resistivity |
Ω/sq |
≤106 |
IEC 62631-3-2 |
|